ARTÍCULO
TITULO

Effect of Microstructure on Corrosion Behavior of Cold Sprayed Aluminum Alloy 5083

Munsu Kim    
Lorena Perez-Andrade    
Luke N. Brewer and Gregory W. Kubacki    

Resumen

This paper investigates the effect of the microstructure on the corrosion behavior of cold sprayed (CS) AA5083 compared to its wrought counterpart. It has been shown that the microstructure of CS aluminum alloys, such as AA2024, AA6061, and AA7075, affects their corrosion behavior; however, investigations of the corrosion behavior of CS AA5083 with a direct comparison to wrought AA5083 have been limited. The microstructure and corrosion behavior of CS AA5083 were examined by scanning electron microscopy (SEM), transmission electron microscopy (TEM), energy dispersive X-ray spectroscopy (EDS), electron backscattered diffraction (EBSD), electrochemical and immersion tests, and ASTM G67. The CS process resulted in microstructural changes, such as the size and spatial distribution of intermetallic particles, grain size, and misorientation. The refined grain size and intermetallic particles along prior particle boundaries stimulated the initiation and propagation of localized corrosion. Electrochemical tests presented enhanced anodic kinetics with high pitting susceptibility, giving rise to extensive localized corrosion in CS AA5083. The ASTM G67 test demonstrated significantly higher mass loss for CS AA5083 compared to its wrought counterpart due to preferential attack within prior particle boundary regions in the CS microstructure. Possible mechanisms of intergranular corrosion (IGC) propagation at prior particle boundary regions have been discussed.

 Artículos similares

       
 
Meng Yao, Qing Wang, Qingbo Yu, Jianzhong Wu, Hui Li, Jiaqi Dong, Weitong Xia, Yan Han and Xinlei Huang    
Artificial reclamation is one of the main means of land expansion in coastal cities. However, the permeability of underlying soft clay (USC), derived from the dredged load, has not been paid enough attention, although it is closely related to the long-te... ver más
Revista: Water

 
Lu Li, Meng Zang, Rongtang Zhang and Haijun Lu    
Consolidated undrained triaxial shear tests were performed on undisturbed saturated structured clay at three unloading rates (0.1, 0.25, and 2.5 kPa/min) using a GDS triaxial system to determine the effects of different unloading rates and unloading stre... ver más
Revista: Buildings

 
Liansheng Tang, Yang Chen, Jialun Peng and Zihua Cheng    
High liquid limit soil has unfavorable engineering geological characteristics, such as strong disintegration, dry shrinkage and easy cracking, and easy uplift when encountering water, which will cause various problems to the engineering. At present, the ... ver más
Revista: Buildings

 
Zuzana Slí?ková, Dita Frankeová and Milo? Drdácký    
The effects of the double and the multiple application (2 to 6) of Calosil® (IBZ-Salzchemie GmbH, Halsbruecke, Germany) E25, IP 25 and E50 products were studied on Maastricht limestone, which is characterized by high porosity and large pores. Both destru... ver más
Revista: Buildings

 
Fernanda Martins Queiroz, Aline de Fátima Santos Bugarin, Victor Hugo Ayusso, Maysa Terada and Isolda Costa    
The AA 2198-T851 is a third-generation Al-Li alloy developed for use in the aircraft industry. Al-Li alloys are susceptible to localized corrosion due to their complex microstructure resulting from the used thermomechanical treatment. In order to prevent... ver más