Carlos Ocampo-Ortega, Ines Riech, Arturo Abelenda, Ricardo Mis-Fernández, Patricia Rodríguez-Fragoso and Julio Mendoza-Alvarez
Tin sulfide (SnS) thin films were deposited by the chemical bath deposition technique. The used procedure allows us to obtain orthorhombic SnS in 3.5 h and achieve thicknesses of 390 nm. We study the influence of deposition times, percentage of Sn precur...
ver más
|
|
|
|
|
|
|
Rui-Wei You, Yen-Pei Fu
Pág. 95 - 98
In this study, ZnS thin films were successfully synthesized by chemical bath deposition (CBD) with starting materials of NH2-NH2, SC(NH2)2, and ZnSO4?7H2O. ZnS thin films were deposited with different time on glass substrates by CBD at 80oC and pH=9. Bas...
ver más
|
|
|
|
|
|
|
Alex Sagalovych,Viktor Popov,Vlad Sagalovych,Stas Dudnik,Roman Popenchuk
Pág. 6 - 15
The process of chemical vapor deposition of Mo and Mo-? coatings was studied by means of thermal decomposition of molybdenum hexacarbonyl. The kinetics of the coating growth in the range of 480 °C?540 °C and the pressure in the reaction volume ...
ver más
|
|
|
|
|
|
|
Jianjun Hu, Chuan He, Xian Yang, Hui Li, Hongbin Xu and Ning Guo
The FeS solid lubricating coatings were prepared on the AISI 5140 steel by chemical bath deposition (CBD) coating technique at various temperatures from 30 to 90 °C. The influence of temperature on microstructure, microcracks, and tribological properties...
ver más
|
|
|
|
|
|
|
Sabah M. Ahmed
Pág. 1 - 9
Introduction: In recent years a metal oxide semiconductors have been paid attention due to their excellent chemical and physical properties. ZnO (Zinc oxide) is considered as one of the most attractive semiconductor materials for implementation in photo-...
ver más
|
|
|
|